·. Uses |
|
| |
Concrete restoration.
Corners and damaged edge restoration.
Concrete restoration in hard conditions (harbours, maritime places, aggressive waters, etc.).
Prefabricated concrete pieces.
Concrete structures restoration.
Concrete hollows repairing.
To repair concrete damaged by a strong impact.
|
|
 |
 |
·. Surface preparation |
|
| |
The surface must be water saturated, clean and exempt of materials of low resistance or badly stuck. Do not apply the product with a room temperature below 5ºC nor over 35ºC. |
|
 |
 |
·. Instructions for use |
|
| |
Mix the product with water at a proportion of 4-5 Lt. per cement bag of 25 Kg. The mixture can be made by hand or by mechanical agitation for 2 or 3 minutes. HORMIDUR 2 must be cured with water or with curing liquid to avoid hydration water evaporation. |
|
 |
 |
·. Consumption |
|
| |
2 Kg. of HORMIDUR 2 per m² and mm. of thickness. |
|
 |
 |
·. Colours |
|
| |
Grey. |
|
 |
 |
·. Packing and storing |
|
| |
HORMIDUR 2 is packed in hermetic barrels; according to EC packing and storing directives for chemical products. |
|
 |
 |
·. Hygiene and safety |
|
| |
See product label. |
|
 |
 |
·. Specification |
|
| |
Aspect: Homogenous grey colour.
Apparent density (at 20ºC):1.35 gr./cm³.approx.
pH :12
Using time at 20ºC: 1 hour.
Concrete adherence: 3 N/mm². 28 days later.
Compression resistance: 45 N/mm². 28 days later.
Flexion resistance: 7 N/mm². 28 days later.
Thickness: 0 – 4 mm.
Sand gradation: < 2 mm.
|
|
 |
| |
NOTES:
- These technical specifications, as the other recommendations and technical information, are useful only for the description of the product characteristics, instructions of use and its uses. Data information are based in our technical knowledge obtained in bibliography, laboratory essays and by our own practice.
- Consumption data and dosages which appears in these specifications are based in our own experience, so they can vary due to different conditions in the building place. Real consumption and dosages have to be determined in the building place through previous essays and they are customer responsibility.
- For further information, our Applied Construction Chemistry Department is at your disposal.
- Other uses witch do not fit with the specifications are not from our responsibility.
- We give guarantee in case of manufacturing quality problems; so excludes further reclamations and our only responsibility is to return the value of the product.
- Patents and rights must be taken into account.